Hard alloy materials for anti adhesive wear
Research and development have been conducted on the adhesive wear that is prone to occur in the processing of high affinity metals such as pure copper and pure iron. By reducing CO and adding special materials, the occurrence of adhesion and sintering can be suppressed. The material maintains high hardness while ensuring sufficient toughness, and also has good resistance to discharge and corrosion.
| series | brand | granularity | Cobalt content (%) | Density (g/cm3) | hardness | Bending strength (Mpa) |
| Anti adhesive wear series | CF40 | 1.3-3.0 | 10 | 14.62 | 89.5 | ≥3200 |
| CE10 | 0.8-6.0 | 6 | 14.95 | 90.0 | ≥3100 |